TOGE concrete screws are not only strong in their anchoring, but also optimally protected against corrosion – thanks to modern zinc flake coatings. We offer a graduated portfolio of high-quality coatings that provide optimum protection against corrosion and are suitable for a wide range of applications. With the TOGE ZFC, TOGE ZFC Solid and TOGE KORR variants, we offer coordinated solutions for different environmental conditions.
Here you will find a compact overview of the properties and advantages of our four materials and main coatings:
The classification into corrosivity categories is based on extensive tests. This gives you a reliable assessment of the duration of protection under real operating conditions – and a good feeling for every decision.
TOGE – The Fastening Experts. Trust in intelligent solutions with proven quality.

Steel, galvanized
| Min. layer thickness | 5 μm |
| Salt spray test according to DIN EN ISO 9227-NSS | 0 hrs. |
| Condensation of water according to DIN EN ISO 6270 | 0 hrs. |
| Corrosion class according to DIN EN ISO 12944 | C1 |
| Duration of protection* | 0 years |

TOGE ZFC
| Min. layer thickness | 6 μm |
| Salt spray test according to DIN EN ISO 9227-NSS | 240 hrs. |
| Condensation of water according to DIN EN ISO 6270 | 120 hrs. |
| Corrosion class according to DIN EN ISO 12944 | C3 – medium |
| Duration of protection* | 7-15 years |

TOGE ZFC Solid
| Min. layer thickness | 17 μm |
| Salt spray test according to DIN EN ISO 9227-NSS | 720 hrs. |
| Condensation of water according to DIN EN ISO 6270 | 480 hrs. |
| Corrosion class according to DIN EN ISO 12944 | C4 – high |
| Duration of protection* | 15-25 years |

TOGE KORR
| Min. layer thickness | 27 μm |
| Salt spray test according to DIN EN ISO 9227-NSS | 4.800 hrs. |
| Condensation of water according to DIN EN ISO 6270 | / |
| Corrosion class according to DIN EN ISO 12944 | C5 ** |
| Duration of protection* |
50 ** years |
* The protection period does not constitute a warranty and is to be understood as the expected service life until the first repair. The component must therefore be accessible and inspectable over the entire period.
** Not according to DIN EN ISO 12944, but according to own test report.
Corrosion class C1:
Heated buildings with a neutral atmosphere.
Corrosion class C3:
Urban and industrial atmosphere with moderate sulphur dioxide pollution.
Corrosion class C4:
Industrial atmosphere and coastal atmosphere with moderate salt exposure.
Corrosion class C5:
Industrial areas with high humidity and aggressive atmosphere. Coastal atmosphere with high salt contamination.
You need to load content from reCAPTCHA to submit the form. Please note that doing so will share data with third-party providers.
More InformationYou are currently viewing a placeholder content from Turnstile. To access the actual content, click the button below. Please note that doing so will share data with third-party providers.
More InformationYou are currently viewing a placeholder content from Facebook. To access the actual content, click the button below. Please note that doing so will share data with third-party providers.
More InformationYou are currently viewing a placeholder content from Instagram. To access the actual content, click the button below. Please note that doing so will share data with third-party providers.
More InformationYou are currently viewing a placeholder content from X. To access the actual content, click the button below. Please note that doing so will share data with third-party providers.
More Information